Publikováno v:
Journal of the Energy Institute. 105:214-220
Autor:
Jiyang Wang, Yu Fu, Wenbo Kong, Shuqing Li, Changkun Yuan, Jieru Bai, Xia Chen, Jun Zhang, Yuhan Sun
Publikováno v:
ACS Catalysis. 12:4382-4393
Autor:
Shuqing Li, Yu Fu, Wenbo Kong, Jiyang Wang, Changkun Yuan, Bingrong Pan, He Zhu, Xia Chen, Yidan Zhang, Jun Zhang, Yuhan Sun
Publikováno v:
Fuel. 343:127918
Autor:
Jieru Bai, Yu Fu, Wenbo Kong, Bingrong Pan, Changkun Yuan, Shuqing Li, Jiyang Wang, Jun Zhang, Yuhan Sun
Publikováno v:
ChemNanoMat. 8
Autor:
Yu Fu, Fufeng Cai, Jun Zhang, Bingrong Pan, Feikai Jin, Jiyang Wang, Wenbo Kong, Yuhan Sun, Changkun Yuan
Publikováno v:
ChemPlusChem. 85(6)
Copper has been incorporated into Ni-Fe alloys to form a series of ternary NiFeCu alloy catalysts with molar ratio of Cu/Fe varying from 0 to 1.5, which were tested in dry reforming of methane (DRM) at 923 K and atmospheric pressure with a CH4 /CO2 r
Publikováno v:
Applied Surface Science. 441:816-823
The Ni/SiO2 catalysts with trace Ru promoter were prepared by either polyethylene glycol (PEG)-assisted or PEG-free impregnation method and were used in CO methanation reaction. The presence of PEG molecules was beneficial to form bimetallic Ni-Ru pa
Publikováno v:
ChemCatChem. 10:2078-2086
Publikováno v:
Journal of Environmental Chemical Engineering. 9:105790
Noble metal nanoparticles (NPs) exhibit high reactivity towards hydrocarbon reforming, however, suffer from agglomeration and poisoning issues (e.g., carbon deposition). A facile and environmental approach to rejuvenate noble metal catalysts is techn
Autor:
Changkun Yuan, Fufeng Cai, Lei Shi, Shuqing Li, Jun Zhang, Evgeny I. Vovk, Wenbo Kong, Xiaohong Zhou, Bingrong Pan, Rui Si, Yuhan Sun, Shenggang Li, Yu Fu, He Zhu, Yong Yang
Publikováno v:
Applied Catalysis B: Environmental. 285:119837
In Ni-catalyzed methane dry reforming (DRM), CH4 tends to dissociate directly to form carbon on Ni nanoparticles. The lack of oxygen availability on the Ni surface easily lead to carbon deposition. Here the precise decoration of Ni surface by SiO2 ca