La Metallurgia Italiana; Issue 7-8, 2009
It is accepted that the majority of surface defects in the continuous casting process originate at, or within 25mm of, the meniscus in the mould. Whether the defects propagate into cracks is dependent on the heat transferdown the remainder of the mou
Autor:
Riaz, S., Ludlow, V., Stewart, B., Smith, A. W., Bell, A., McDonald, M., Burniston, R., Hopkins, M., van der Knoop, W., Stamp, D., Ferguson, A.
Publikováno v:
Ironmaking & Steelmaking; Sep2007, Vol. 34 Issue 5, p403-409, 7p