Publikováno v:
In Engineering Failure Analysis December 2019 106
Publikováno v:
In Procedia Structural Integrity 2018 13:2216-2220
Publikováno v:
In Procedia Structural Integrity 2018 13:2221-2226
Publikováno v:
In Procedia Materials Science 2014 3:1429-1434
Publikováno v:
In Materials and Design February 2013 44:303-310
Publikováno v:
Journal of Mining and Metallurgy. Section B: Metallurgy, Vol 46, Iss 1, Pp 25-32 (2010)
Many of modern technologies require materials with unusual combinations of properties that cannot be met by the conventional metal alloys, ceramics, and polymeric materials. Material property combinations and ranges have been extended by the developm
Externí odkaz:
https://doaj.org/article/c386c47f6f8b4f67b462cc04fd94ce44
Autor:
Perković S; Military Technical Institute, 11000 Belgrade, Serbia., Sedmak A; Faculty of Mechanical Engineering, University of Belgrade, 11120 Belgrade, Serbia., Radaković Z; Faculty of Mechanical Engineering, University of Belgrade, 11120 Belgrade, Serbia., Burzić Z; Military Technical Institute, 11000 Belgrade, Serbia., Sedmak S; Innovation Centre, Faculty of Mechanical Engineering, 11120 Belgrade, Serbia., Radović L; Military Technical Institute, 11000 Belgrade, Serbia., Mandić J; Military Technical Institute, 11000 Belgrade, Serbia.
Publikováno v:
Materials (Basel, Switzerland) [Materials (Basel)] 2023 Jun 16; Vol. 16 (12). Date of Electronic Publication: 2023 Jun 16.
Publikováno v:
Metalurgija, Vol 46, Iss 2, Pp 87-92 (2007)
Results of the experimental and numerical comparative analysis of steamline pipes have been presented. New pipes and the pipes used for more than 117,000 hours at 540 °C under pressure of 42 bars have been simultaneously tested. This testing has bee
Externí odkaz:
https://doaj.org/article/a05fc5fc8c664b9e827656cf91f3e165
Publikováno v:
Metalurgija, Vol 46, Iss 4, Pp 237-243 (2007)
The resistivity of a coarse grain steel against fatigue crack initiation in presence of micro-defects is discussed. Samples of material with martensitic microstructure were prepared by adequate thermal treatment. Microstructurally small Vickers inden
Externí odkaz:
https://doaj.org/article/dd3229bb7a2b4a7d91a60e79ad02ef76
Publikováno v:
In Materials and Design 2010 31(4):1790-1798