Publikováno v:
Metals, Vol 12, Iss 4, p 661 (2022)
High silicon and molybdenum (SiMo) ductile iron is commonly used for car exhaust systems, and its micro-structural dispersity depends on intrinsic parameters, which include alloy composition and inoculation efficiency, as well as extrinsic factors, s
Externí odkaz:
https://doaj.org/article/02deb045d4074fec9bff1b4a86ae295f
Autor:
Semen Naumovich Lekakh, Larry Godlewski, Ronald J. O'Malley, Asebi Bofah, Richard Osei, Mei Li
Publikováno v:
Oxidation of Metals. 95:251-268
Silicon and molybdenum (SiMo) alloyed cast irons with spherical graphite are used for exhaust manifolds for service at high temperatures in air and combustion atmospheres containing water vapor. Analysis of degraded surfaces of in-service manifolds i
Publikováno v:
Metallurgical and Materials Transactions B. 51:2542-2554
High silicon molybdenum-alloyed cast irons (SiMo) with spherical graphite are widely used for cast thin-wall exhaust manifolds, worked in high-temperature oxidation environment; therefore, prevention of surface degradation during service is important
Publikováno v:
International Journal of Metalcasting. 15:874-888
High alloyed Si ferritic ductile irons can offer potential benefits because they combine high strength, ductility at room temperature, and low oxidation rate at high temperature. However, there is one known drawback and that is these cast irons have
Publikováno v:
Oxidation of Metals. 94:251-264
High SiMo cast iron components in automotive exhaust systems are exposed to high-temperature oxidation over time. Quantitative analysis of formed oxide scale is therefore important for the assessment of a component durability. The brittle nature of m
Publikováno v:
International Journal of Metalcasting. 15:889-889
In the original version of the article, Fig. 4b was processed incorrectly by the publisher. Following is the correct Fig. 4. The original article has been updated.