Grinding is often used for machining because it allows for high dimensional and shapes accuracy as well as low surface roughness. Modern technologies of grinding steel with ferritic-pearlitic structure combine the cutting process with simultaneous su
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::8fcc516f5fff94a2106da4e7dd6f9056
https://doi.org/10.21203/rs.3.rs-1994356/v1
https://doi.org/10.21203/rs.3.rs-1994356/v1
Publikováno v:
International Journal of Precision Engineering and Manufacturing-Green Technology. 9:175-190
The article contains the results of tests on a laser-processed eyelet of undercarriage drag strut to increase its fatigue strength. Laser processing concentrated on both sides around the hole of eye for connecting the undercarriage drag strut caused
Autor:
Małgorzata Grabara, Anna Bieniec
Publikováno v:
PeerJ, Vol 12, p e18092 (2024)
Background Understanding the relationship between the functional state of the musculoskeletal system and skating performance in ice hockey players is essential, as it can provide valuable insights for the development of training programs tailored to
Externí odkaz:
https://doaj.org/article/8c22e08432b2476eaa1366262364d5bd
Publikováno v:
Chinese Journal of Aeronautics, Vol 32, Iss 3, Pp 701-714 (2019)
This paper presents the results of material characterization and a fatigue test conducted for a laser-re-melted drag strut used in an aircraft landing gear. The drag strut was re-melted with a CO2 laser beam. Eight re-melted paths were made in the fo
Autor:
Katarzyna Zdziebło, Urszula Łapińska, Ewelina Machała-Ćwikła, Piotr Zdzieblo, Piotr Ćwikła, Anna Zdziebło, Anna Bieniasz, Dominika Machała, Kamila Machała
Publikováno v:
Quality in Sport, Vol 17 (2024)
A fatigue fracture, also known as stress fracture or overuse fracture, is caused by the summation of micro-injuries resulting from a chronic state of bone overload. It affects 1.4 %- 4.4 % of professional athletes. The most common site of fatigue fra
Externí odkaz:
https://doaj.org/article/66f027476b95475c887837dbe8734dd1
Autor:
Piotr Zdzieblo, Ewelina Machała-Ćwikła, Urszula Łapińska, Piotr Ćwikła, Kamila Machała, Anna Zdziebło, Dominika Machała, Katarzyna Zdzieblo, Anna Bieniasz
Publikováno v:
Quality in Sport, Vol 17 (2024)
The utility of cannabinoids as agents used to treat diseases is a popular topic of discussion these days. The approval of medical marijuana continues to stir up controversy. As far back as ancient times, hemp was used for medicinal purposes. These pl
Externí odkaz:
https://doaj.org/article/f30c0b4fbbe44c6fbb91089383af4acc
Autor:
Blanka Wolszczak-Biedrzycka, Anna Bieńkowska, Beata Cieślikiewicz, Elwira Smolińska-Fijołek, Grzegorz Biedrzycki, Justyna Dorf
Publikováno v:
Annals of Medicine, Vol 55, Iss 1, Pp 722-732 (2023)
AbstractAim A third (booster) dose of the anti-SARS-CoV-2 vaccine became necessary due to the observed decrease in anti-SARS-CoV-2S antibody levels over time, new mutations, and low global vaccination rates. In this study, anti-SARS-CoV-2S antibody l
Externí odkaz:
https://doaj.org/article/6af4a9d187cf4f14b9e29be0b5f58ceb
Publikováno v:
Ceramics International. 42:11275-11284
Commercially available austenic stainless steel substrate was coated with commercially available, raw Al2O3 powder applied by means of plasma spraying method and then re-melted with CO2 laser beam of various parameters. Tribological and mechanical pr
Autor:
Marek Szkodo, Anna Bień
Publikováno v:
Surface and Coatings Technology. 296:117-123
The paper contains the results of the structural analysis, hardness tests and fatigue tests conducted for the medium carbon structural steel with low content of Cr and Ni after its processing with CO 2 laser beam. Pre-cracks were made in the round co
Autor:
Marek Szkodo, Anna Bień
Publikováno v:
Journal of Materials Processing Technology. 217:114-121
The paper presents the results of laser-melted C80U steel. The processed steel was placed between two permanent magnets and laser beam whose scanning velocity was 10 mm/s. CO 2 laser beam was working in pulse mode. Pulses were generated at 100% of th