Dry storage canisters of used nuclear fuels are fabricated using SUS 304L stainless steel. Chloride-induced stress corrosion cracking (CISCC) is one of the major failure modes of dry storage canisters. The cracked canisters can be repaired by frictio
Externí odkaz:
https://doaj.org/article/de816451048841ff8375f02b2e6ffd57
Autor:
Anirban Naskar, Madhumanti Bhattacharyya, Krishnan S. Raja, Indrajit Charit, Jens Darsell, Saumyadeep Jana
Publikováno v:
Corrosion Engineering, Science and Technology. 57:599-612
Publikováno v:
Transactions of the Indian National Academy of Engineering. 7:197-205
Extensive research on additive manufacturing (AM) has revealed its potential as well as its limitations. The components produced by AM usually do not meet the standard for direct end-use due to poor dimensional tolerance and surface finish. Therefore
Publikováno v:
Journal of Manufacturing Processes. 36:44-50
Inconel 718 (IN 718) is one of the important nickel based alloys that is being extensively used in aerospace industry. Being an aerospace material, surface integrity is of paramount importance due to high risk factor involved in this kind of industry
Autor:
Anirban Naskar, Jens T. Darsell, Madhumanti Bhattacharyya, Krishnan S. Raja, Indrajit Charit, Saumyadeep Jana
Publikováno v:
SN Applied Sciences. 2
Stainless steel (SS) canisters used for storing spent nuclear waste are prone to chloride-induced stress corrosion cracking. Friction stir welding (FSW), being a low heat input process, can be used for repair welding of these canisters. In this study
Autor:
Anirban Naskar, S. Paul
Publikováno v:
NDT & E International. 126:102592
Publikováno v:
Ceramics International. 44:17013-17021
Exceptional properties of advanced ceramics attract various heavy engineering industries. But surface and sub-surface defects generated during final stage abrasive machining processes make them vulnerable and limit their widespread use. This study ai
Publikováno v:
Journal of Manufacturing Processes. 35:624-633
Ceramics are the most sought-after materials in various advanced engineering applications. Diamond abrasive machining is used to achieve dimensional tolerances for hard ceramic materials. Micro-brittle fracture and grain dislodgement are the primary
Publikováno v:
Advances in Materials and Processing Technologies. 4:626-638
Investigations on the grindability of titanium alloy with conventional wheel were mostly limited to a wheel speed of 30 m/s. Even with the monolayer electroplated cBN wheel, most of the experiments were limited to a wheel speed of 30 m/s. Surface res
Autor:
Anirban Naskar, A.K. Chattopadhyay
Publikováno v:
Wear. :98-106