Zobrazeno 1 - 8
of 8
pro vyhledávání: '"Andrej Likeb"'
Autor:
Andrej Likeb, Nenad Gubeljak
Publikováno v:
Metals, Vol 10, Iss 6, p 749 (2020)
To estimate the acceptable size of cracks and predict the loading limit of the pipeline or its resistance to the initiation and crack growth by following the structural integrity, the fracture toughness and limit load solutions are required. Standard
Externí odkaz:
https://doaj.org/article/3696381746f04f949344840d31edb645
Autor:
Nenad Gubeljak, Andrej Likeb
Publikováno v:
Metals
Volume 10
Issue 6
Metals, Vol 10, Iss 749, p 749 (2020)
Volume 10
Issue 6
Metals, Vol 10, Iss 749, p 749 (2020)
To estimate the acceptable size of cracks and predict the loading limit of the pipeline or its resistance to the initiation and crack growth by following the structural integrity, the fracture toughness and limit load solutions are required. Standard
Publikováno v:
Archive of Applied Mechanics. 89:897-909
For safe transport and reliable supply of petrochemical substances, it is crucial to ensure the structural integrity of the equipment, pipelines in particular. Regarding the large diameters and high mass per distance, pipelines for natural gas are de
Autor:
Ivana Cvijović-Alagić, W. Musraty, Andrej Likeb, Aleksandar Sedmak, Nenad Gubeljak, Bojan Medjo, Marko Rakin
Publikováno v:
Engineering Fracture Mechanics
Integrity of pipes is typically assessed by testing fracture mechanics specimens, such as compact tensile (CT) or single-edge notched bending (SENB). However, for some pipe dimensions it is not easy or possible to fabricate a specimen conforming to t
Publikováno v:
Fatigue & Fracture of Engineering Materials & Structures. 37:1319-1329
The object of this paper is to develop the load separation method for the new pipe-ring notched bend specimen. The paper presents an approach for determining the plastic load line displacement (ηpl LLD ) and the plastic crack mouth opening displacem
Publikováno v:
Procedia Materials Science. 3:1934-1940
Fracture toughness Measurement of thin walled pipe-line with flaw or defect in most critical axial direction is difficult. In this paper the non-standard modified specimens has been proposed for simple fracture testing. The comparison between fractur
Publikováno v:
Procedia Materials Science. 3:1941-1946
Pipelines are often designed as thin walled structure, where the standard specimen for fracture toughness testing is difficult to cut. Most critical crack orientation is in axial direction, because the hoop stress is two times higher than radial one.
Publikováno v:
Key Engineering Materials. :637-640
Thethin walled structures as pipe-line are often unsuitable for standard testingof fracture toughness. One possibility is applying non-standard modifiedspecimens with simple testing procedure, but measured fracture behaviour isconsequence of loading