AIP Advances, Vol 8, Iss 4, Pp 047705-047705-5 (2018)
Equiatomic FeCo alloys with average particle size of 24 μm were sintered using spark plasma sintering (SPS) system at sintering temperatures of 1100, 800, and 850 °C for heating rates 50, 100, 300 °C/min by applying pressure of 50 MPa instantly at
Externí odkaz:
https://doaj.org/article/f56e6ee51aa8497c921f196defc9fa3e
Publikováno v:
Air Quality, Atmosphere, & Health
Novel corona virus (COVID-19) pandemic in the last 4 months stimulates the international scientific community to search for vaccine of antiviral agents suitable for in activating the virus inside and outside the human body. More than 4 million people
Autor:
Ali A. Jazie, Amar J. Albaaji
Publikováno v:
JOM.
Reuse of waste such as eggshells and animal bones as a catalyst to convert waste cooking oil into biodiesel fuel was investigated. A mixture of bone and eggshell waste (50:50) was used as a catalyst for biodiesel production from waste cooking oil. Di
Publikováno v:
Materials & Design, Vol 122, Iss, Pp 296-306 (2017)
Carbon nanotubes (CNTs) reinforced FeCo alloys were produced by high energy ball-milling and spark plasma sintering (SPS). CNTs distribution in the FeCo alloy was gradually improved as ball-milling time increased, with a uniform dispersion achieved a
Publikováno v:
Journal of Materials Research. 31:3448-3458
Different volume fractions (0.5 vol. % to 4.5 vol. %) of CNTs were used to reinforce a binary Fe50Co soft magnetic alloy. The first method for dispersion was involved dry mixing and ball milling of the powder, while the second was included wet mixing
Publikováno v:
Journal of Materials Science. 51:7624-7635
The effect of the addition of graphene nanoplatelets (GNP) and graphene nanoplatelet/carbon nanotube (GNT) mixtures on the mechanical and magnetic properties of spark plasma sintered soft magnetic FeCo alloys was studied. Three different volume fract
Equiatomic FeCo alloys were densified using spark plasma sintering (SPS). Using a constant 50 MPa pressure, the sintering temperature and dwell times for the SPS process were optimised for different heating rates (50, 100, 300 °C min−1). All sampl
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::a4fe12954ec745a635b94091d478b482
https://orca.cardiff.ac.uk/id/eprint/103380/3/manuscript.pdf
https://orca.cardiff.ac.uk/id/eprint/103380/3/manuscript.pdf
Publikováno v:
AIP Advances, Vol 8, Iss 4, Pp 047705-047705-5 (2018)
Equiatomic FeCo alloys with average particle size of 24 μm were sintered using spark plasma sintering (SPS) system at sintering temperatures of 1100, 800, and 850 °C for heating rates 50, 100, 300 °C/min by applying pressure of 50 MPa instantly at
Publikováno v:
Journal of Materials Science. Nov2017, Vol. 52 Issue 22, p13284-13295. 12p. 2 Black and White Photographs, 3 Charts, 7 Graphs.
Publikováno v:
Journal of Materials Science. Aug2016, Vol. 51 Issue 16, p7624-7635. 12p.