Publikováno v:
Advanced Materials Research. 1109:419-423
The polymer of poly (3-hexylthiophene) was active layer in application such as solar cells. In this paper, P3HT has been chosed to know the effect of temperature onto P3HT. The optical properties of P3HT were measured by using photoluminescence spect
Publikováno v:
Applied Physics A. 116:2119-2124
Electrical impedance characteristics of porous silicon nanostructures (PSiNs) in frequency function were studied. PSiNs were prepared through photo-electrochemical etching method at various current densities (15–40 mA/cm2) and constant etching time
Publikováno v:
Advanced Materials Research. 832:562-566
Lanthanum Phosphate (LaPO4) nanostructures thin films have been successfully synthesized by sol-gel spin coating technique from lanthanum nitrate and ammonium phosphate in ammonia solution. The procedure starting with formation of homogenous and tran
Publikováno v:
Advanced Materials Research. 832:585-588
Thins films of lanthanum phosphate (LaPO4) were fabricated on glass substrate using successive layer by layer (LbL) assembly method subsequent with furnace annealing. Lanthanum Phosphate (LaPO4) thin films were prepared through sol gel and spin coati
Publikováno v:
Advanced Materials Research. 832:557-561
The electrical properties of Cadmium Selenium (CdSe) nanoparticles were measured by using I-V characteristic under illumination of light (AM 1.5, 100mWcm-2) at room temperature. The cadmium chloride (CdCI) as the Cd precursor and selenium (Se) powder
Publikováno v:
Advanced Materials Research. 832:827-831
Cadmium Selenide (CdSe) was obtained by using spray-deposited method which is using the sodium selenosulfite as Se precursor and cadmium chloride (CdCI) as cadmium (Cd) precursor. Time for each spray-deposited was used as the main parameter to invest
Publikováno v:
Advanced Materials Research. 832:649-653
In this work, titanium Dioxide (TiO2) powder was prepared by sol gel method using Titanium (IV) Isopropoxide (TTIP) as precursor and Ethanol (C2H5OH) as solvent. The sol-gel was heated at temperature 150°C in 1 hour. Titanium Dioxide (TiO2) powder w
Publikováno v:
Advanced Materials Research. 667:68-73
The present paper reports on the structural properties of Lanthanum Phosphate (LaPO4) nanostructure film in term of its surface morphology. In this study, the LaPO4 samples were prepared by sol-gel spin coating method with different layers. Photolumi
Publikováno v:
Advanced Materials Research. 626:302-305
LaPO4 particles with different morphologies and sizes have been successfully synthesized via sol-gel spinned coating process. The aim of this paper is to investigate the effect of annealing on the morphology and formation of LaPO4 on thin films. Phys
Publikováno v:
International Journal of Materials Engineering Innovation. 7:33
Multi-walled carbon nanotubes (MWCNs) were synthesised using double-furnace thermal chemical vapour deposition technique at 700-900°C on porous silicon nanostructure (PSiNs). Palm oil was used as a carbon natural source, ferrocene as a catalyst and