Zobrazeno 1 - 7
of 7
pro vyhledávání: '"A. I. Gaydar"'
Autor:
V. N. Pimenov, I. V. Borovitskaya, A. S. Demin, N. A. Epifanov, E. E. Kazilin, S. V. Latyshev, S. A. Maslyaev, E. V. Morozov, I. P. Sasinovskaya, G. G. Bondarenko, A. I. Gaydar
Publikováno v:
Inorganic Materials: Applied Research. 13:1238-1246
Autor:
V. N. Pimenov, I. V. Borovitskaya, V. A. Gribkov, A. S. Demin, N. A. Epifanov, S. A. Maslyaev, E. V. Morozov, I. P. Sasinovskaya, G. G. Bondarenko, A. I. Gaydar, M. Paduch
Publikováno v:
Journal of Surface Investigation: X-ray, Synchrotron and Neutron Techniques. 16:33-41
Autor:
A. V. Golikov, A. K. Dulatov, S. A. Maslyaev, E. V. Morozov, V. N. Pimenov, G G Bondarenko, A. S. Demin, I. V. Borovitskaya, Vladimir A. Gribkov, A. I. Gaydar
Publikováno v:
Instruments and Experimental Techniques. 63:68-76
A Vikhr plasma-beam device of the Dense Plasma Focus (DPF) type with an energy of ~5 kJ has been recently put into operation at the Baikov Institute of Metallurgy and Material Science. The device, the design of its components, and its parameters are
Autor:
V. A. Gribkov, S. A. Maslyaev, A. I. Gaydar, E. V. Morozov, A. S. Demin, V. N. Pimenov, I. V. Borovitskaya, Gennady G. Bondarenko
Publikováno v:
Industrial laboratory. Diagnostics of materials. 85:29-36
Autor:
V. N. Pimenov, A. I. Gaydar, N. A. Epifanov, Marian Paduch, V. P. Sirotinkin, S. A. Maslyaev, I. P. Sasinovskaya, Vladimir A. Gribkov, G. S. Sprygin, Gennady G. Bondarenko, E. V. Dyomina
Publikováno v:
Inorganic Materials: Applied Research. 10:503-511
The damage and structural state of the surface layer of Al–Li–Mg samples composed of Al–5% Mg–2% Li (wt %) under pulsed action of power streams of high-temperature deuterium plasma and high-energy deuterium ions in the Plasma Focus (PF) devic
Autor:
E. E. Kazilin, E. V. Morozov, S. A. Maslyaev, A. G. Kol’tsov, V. N. Pimenov, S. V. Latyshev, G G Bondarenko, V. V. Roshchupkin, E. V. Demina, A. S. Demin, Vladimir A. Gribkov, A. I. Gaydar
Publikováno v:
Inorganic Materials: Applied Research. 9:361-369
The degradation of a bilateral pressed tungsten surface layer by pulsed laser irradiation in the free-running mode (power density q = 105–5 × 106 W/cm2, pulse duration τ = 0.7 ms) and the Q-switched mode (q = 109–1010 W/cm2, τ = 80 ns) as well
Autor:
S. V. Kucherenko, S. A. Pozidaeva, A. I. Gaydar, A. S. Astahov, V. M. Narochnaya, T. V. Lipkina, S. M. Lipkin, E. I. Kucherenko, V. G. Shishka
Publikováno v:
Kontrol'. Diagnostika.. :45-54