Publikováno v:
Metals, Vol 9, Iss 5, p 594 (2019)
Hybrid laser-arc welding offers many advantages, such as deep penetration, good gap bridge-ability, and low distortion due to reduced heat input. The filler wire which is supplied to the process is used to influence the microstructure and mechanical
Externí odkaz:
https://doaj.org/article/3a5ce2888bc4425a84223673840932e5
Autor:
Xiangmeng Meng, Antoni Artinov, Marcel Bachmann, Ömer Üstündağ, Andrey Gumenyuk, Michael Rethmeier
Element transport in the wire feed laser beam welding (WFLBW) is directly determined by the molten pool shape and thermo-fluid flow therein. In this paper, an untypical molten pool profile, i.e., elongated at its top and bottom but narrowed at the mi
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::2bfa1a1a8da782f991fab213029c81c8
https://depositonce.tu-berlin.de/handle/11303/17145
https://depositonce.tu-berlin.de/handle/11303/17145
Publikováno v:
Welding in the World. 64:501-511
The aim of the present study is to investigate the influence of the laser hybrid welding parameters on the solidification cracks in the weld root for partial penetration welding. Welding trials were performed on thick-walled high-strength steels of g
Publikováno v:
Procedia CIRP. 94:293-297
The development of high energy laser sources enables single-pass welds of thick plates up to 30 mm, but often additional materials are needed to influence the properties of the weld seams. However, the homogenous distribution of filler materials in f
Publikováno v:
Procedia CIRP. 94:676-679
The study deals with the application of the high-power hybrid-laser arc welding process on up to 15 mm thick pipe segments with the intention to avoid end crater imperfections during closing of the circumferential welds, where the pipes were turned d
Publikováno v:
Welding in the World. 64:407-417
The present work deals with the development of a strategy for the prevention of end crater defects in high-power laser welding of thick-walled circumferential welds. A series of experiments were performed to understand the influence of the welding pa
Publikováno v:
Procedia Manufacturing. 36:112-120
The presented study deals with the performing and mechanical testing of single pass hybrid laser-arc welds (HLAW) on 25 mm thick plates made of steel grade S355J2. One of the challenges have to be solved at full penetration HLAW of thick plates is th
Autor:
Cristina Churiaque, Andrey Gumenyuk, Ömer Üstündağ, M. Porrua-Lara, Michael Rethmeier, José María Sánchez-Amaya
Publikováno v:
Optics & Laser Technology 143 (2021) 107284
RODIN. Repositorio de Objetos de Docencia e Investigación de la Universidad de Cádiz
instname
RODIN: Repositorio de Objetos de Docencia e Investigación de la Universidad de Cádiz
Universidad de Cádiz
RODIN. Repositorio de Objetos de Docencia e Investigación de la Universidad de Cádiz
instname
RODIN: Repositorio de Objetos de Docencia e Investigación de la Universidad de Cádiz
Universidad de Cádiz
One of the main concerns in the early stages of manufacturing flat units of shipbuilding is to ensure the quality of the joints throughout the structure. The flat units are constituted by butt welded flat plates, on which longitudinal T-welded reinfo
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::f6a812e62e00063c8dc7cc17e3ff5f62
http://hdl.handle.net/10498/24929
http://hdl.handle.net/10498/24929
One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The s
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::a169cc95ac5c9c80197b8f7c2dbc76f9
Hybrid laser-arc welding of thick-walled ferromagnetic steels with electromagnetic weld pool support
Publikováno v:
Welding in the World. 62:767-774
The hybrid laser-arc welding (HLAW) process provides many advantages over laser welding and arc welding alone, such as high welding speed, gap bridgeability, and deep penetration. The developments in hybrid laser-arc welding technology using modern h