Zobrazeno 1 - 10
of 10
pro vyhledávání: '"É. L. Kolosova"'
Publikováno v:
Metal Science and Heat Treatment. 33:294-299
1. An agent based on polymer Na-CMC is more sensitive to an increase in temperature than an agent based on PK-2. An increase in aqueous Na-CMC solution temperature leads to a marked reduction in the heat removal coefficient in the pearlitic transform
Publikováno v:
Metal Science and Heat Treatment. 32:829-834
1. to obtain a satisfactory distribution of cooling rates in PK-2 media, it is necessary to observe the following procedure for medium preparation prior to quenching; aging of the concentrate by immersing heated metal in the bath to raise the tempera
Autor:
A. V. Evdokimov, Gordienko Mikhail S, É. L. Kolosova, V. A. Palyanichka, I. G. Volkov, V. D. Roztorguev
Publikováno v:
Metallurgist. 25:90-93
Publikováno v:
Metal Science and Heat Treatment. 30:778-781
1. A reduction in the level of impact strength for quenched and tempered steel on introducing vanadium and titanium into it is caused by cementite platelet thickening and presence of dispersed V(C, N) and TiN particles. Microalloying with zirconium i
Publikováno v:
Metal Science and Heat Treatment. 15:650-653
1. The morphology and dislocation arrays in excess ferrite vary with the transformation temperature and holding time. 2. At 700 and 650° ferrite is precipitated largely in the grain boundaries. At 650° sections of Widmanstatten ferrite appear after
Reduction in oxide stringer content of rails by deoxidizing rail steel with FeSiCa and FeSiZr alloys
Publikováno v:
Metallurgist. 25:61-63
More difficult service conditions for railroad rails means that the quality of the rails must continually be improved. One of the most important aspects of this problem is reducing the degree of contamination of the rails with stringer-type oxide inc
Autor:
V. E. Semenkov, V. I. Syreishchikova, I. Ya. Vinokurov, A. B. Dobuzhskaya, É. L. Kolosova, A. A. Deryabin
Publikováno v:
Metallurgist. 24:436-438
Autor:
I. Ya. Vinokurov, N. A. Loshkina, E. M. Murav'ev, A. V. Evdokimov, V. I. Syreishchikova, É. L. Kolosova
Publikováno v:
Metallurgist. 24:441-443
Autor:
V A Baranova, V. I. Syreishchikova, A. V. Evdokimov, I Y Vinokurov, D M Rabinovich, É. L. Kolosova
Publikováno v:
Metallurgist. 20:617-618
Contact fatigue cracks are the main type of failure in rails. The large streak inclusions of alumina formed as a result of deoxidizing the steel in the ladle with aluminum are dangerous as regards formation of fatigue defects. These harmful inclusion
Autor:
V. E. Semenkov, A. B. Dobuzhskaya, V. I. Syreishchikova, A. V. Pan, M. A. Stambul'chik, É. L. Kolosova, A. A. Deryabin
Publikováno v:
Metallurgist. 32:382-383
It is known that the deoxidation of rail steel in the ladle with complex ferroalloys based on silicon and including calcium, magnesium, titanium, Or zirconium in a certain combination makes it possible to obtain railroad rails of group-I quality char