Zobrazeno 1 - 10
of 49
pro vyhledávání: '"623"'
Publikováno v:
Journal of Alloys and Compounds. 800:343-354
A lean Mg–Zn–Al alloy has been developed through melting-casting and subsequently thermomechanically processed within the temperature range of 523 K–723 K, by employing a novel ‘hard plate hot forging’ method. The elevated temperature defor
Publikováno v:
Surface and Coatings Technology. 372:1-8
A high-intensity metal ribbon ion beam was generated using plasma immersion extraction and the acceleration of the metal ions with their subsequent ballistic focusing using a cylindrical grid electrode under a repetitively pulsed bias. To generate th
Publikováno v:
Materials Today: Proceedings. 47:665-667
The study of thermoelectric materials, which convert thermal energy to electrical energy in the solid state, has grown immensely in the past decade. The polycrystalline Ca3Co4O9 powder were synthesized using conventional sold state route by employing
Publikováno v:
Journal of Alloys and Compounds. 788:338-344
Zn powder was mixed with Cu nanoparticle joints by applying a very low additional pressure of 20 kPa to improve the bonding strength. Cu-Zn alloying throughout the bonding layer was achieved by firing at 623 K for 5 min. The phase composition of the
Publikováno v:
Journal of Alloys and Compounds. 767:253-258
The thermal stability of microstructures induced by laser shock peening (LSP) in TC17 titanium alloy (Ti-5Al-2Sn-2Zr-4Mo-4Cr) was investigated by comparing the microstructural characteristics and mechanical properties, which were characterized by tra
Publikováno v:
Journal of Alloys and Compounds. 741:1222-1228
Mg-0.80Ce-0.69Zn-0.03Zr (wt %) alloys were prepared in the state of as-cast, by homogenization treatment at 713 K for 12 h and extruded at 573 K, 623 K, and 673 K with an extrusion ratio of 10.24: 1. Experimental results reveal that the grains are re
Publikováno v:
Intermetallics. 93:338-342
Achieving high power factor values for BiSbTe alloys is important for further elevation of their thermoelectric performance. In this report, Bi 0.4 Sb 1.6 Te 3 bulk samples were prepared by a fusion method followed by hot pressing at different temper
Publikováno v:
Materials Characterization. 172:110885
In the present investigation, annealing treatment at a temperature of 623 K for 5 min has been carried out on Mg-4Zn-0.5Ca-0.16Mn (wt%) alloy specimens forged at various temperatures viz., 523 K, 573 K, and 623 K. Furthermore, the specimen forged at
Publikováno v:
Rare Metal Materials and Engineering. 46:1491-1496
To evaluate the mechanical properties and promote a better understanding of failure behavior of the newly developed Zr-Nb cladding tubes during reactivity initiated accidents (RIAs), burst tests were carried out with the biaxial stress state under di
Publikováno v:
Journal of Manufacturing Processes. 26:178-187
Dissimilar metal joints have some advantages such as high functionality characteristics for the industrial usage. This paper describes the effect of friction welding condition on joining phenomena, tensile strength, and bend ductility of friction wel