Metals, Vol 7, Iss 12, p 544 (2017)
Metals; Volume 7; Issue 12; Pages: 544
Metals; Volume 7; Issue 12; Pages: 544
The influence of combined (helical and pass) rolling on the structure, residual porosity, and microhardness of an AA6082-0.2 wt % Al2O3 composite produced by casting with ultrasonic processing was evaluated in comparison with the matrix alloy. The na
Publikováno v:
Metals, Vol 7, Iss 12, p 544 (2017)
The influence of combined (helical and pass) rolling on the structure, residual porosity, and microhardness of an AA6082-0.2 wt % Al2O3 composite produced by casting with ultrasonic processing was evaluated in comparison with the matrix alloy. The na