Zobrazeno 1 - 10
of 33
pro vyhledávání: '"91"'
Publikováno v:
Journal of Crystal Growth. Jul2021, Vol. 565, pN.PAG-N.PAG. 1p.
Autor:
Liang Li1, Defang Duan1, Qiang Zhou1, Dapeng Xu1, Tian Cui1 tiancui@jlu.edu.cn, Bingbing Liu1, Hongming Yuan2
Publikováno v:
Journal of Crystal Growth. Sep2014, Vol. 402, p109-112. 5p.
Autor:
Hao, Z.1 hao@istec.or.jp, Wu, Y.1, Enomoto, Y. enomoto@istec.or.jp, Tanabe, K.1, Koshizuka, N.1
Publikováno v:
Journal of Crystal Growth. Feb2002, Vol. 235 Issue 1-4, p253. 5p.
Autor:
M. Czupalla, Peter Rudolph, F. Kirscht, Wolfram Miller, B. Lux, Martin Albrecht, Ch. Frank-Rotsch
Publikováno v:
Journal of Crystal Growth. 318:249-254
Conventionally grown Czochralski (Cz) silicon crystals for photovoltaic (PV) application have an unfavourable cylindrical shape leading to essential material loss during the wafer cutting process. Additionally, the typical high oxygen concentration p
Publikováno v:
Journal of Crystal Growth. 565:126150
In this paper the growth of a 16mm diameter Ce-doped Tl$_2$NaYCl$_6$ and its characterization as a gamma-ray detector are reported. With a 16 mm dia. x 8 mm cylindrical sample, energy resolution of 4.1% (FWHM) at 662 keV and light yield of 27,800ph/M
Publikováno v:
Journal of Crystal Growth. 402:109-112
Mg 4 Nb 2 O 9 single crystals were prepared by the optical floating zone method. While the as-grown were boules polycrystalline and cracked with dimensions of ∅ 5–8 mm× L 91 mm, they contained single crystal regions as large as ∅ 4 mm× L 15 m
Autor:
Jong Yeog Son, W.J. Maeng
Publikováno v:
Journal of Crystal Growth. 363:105-108
Epitaxial (001) BiFeO 3 thin films with tetragonally stained structures and a c / a ratio of about 1.04 were fabricated on single crystalline (100) Rh substrates. The BiFeO 3 thin film showed high remanent polarization ( P r ) of about 91 μC/cm 2 .
Publikováno v:
Journal of Crystal Growth. 311:2470-2473
In this paper, we report on the improved scintillation properties of Cs 2 NaCeCl 6 crystal. The Cs 2 NaCeCl 6 crystal was grown by the Czochralski technique in the dimensions of ⊘10×4 mm 3 . X-ray excited luminescence measurements of the Cs 2 NaCe
Publikováno v:
Journal of Crystal Growth. 310:1401-1404
Effects of the growth velocity on the crystal growth behavior of Bi_2Sr_2Ca_1Cu_2O_x (Bi-2212) have been studied by floating zone technique. The results show that a necessary condition for obtaining large single crystals along the c-axis is that the
Publikováno v:
Journal of Crystal Growth. 235:253-257
Extremely smooth single crystal YBa 2 Cu 3 O 7− δ “thin” films, 1–3 μm thick, have been successfully grown on YBCO-seeded MgO substrates by liquid phase epitaxy. The morphology study on the as-grown samples has revealed a step-flow growth m